Hello, the team has never had a chance to use such products. But from the formula composition,
Bis-PEG-18 Methyl Ether Dimethyl Silane is used.
Bis-PEG-18 Methyl Ether Dimethyl Silane at a relatively large rate, probably about 5%, helps to adjust the contact surface. As for the silicone in the Estee ANR formula, no silicone other than
Bis-PEG-18 Methyl Ether Dimethyl Silane . Use other silicones in the formula as well. The surface should be more slippery. The original product, and other elements in the formula also affect the texture of the skin. And there is a chance that the member's formula Might be gooier with more elements between
Laurocapram and DMI, please choose one only. Because it will not work redundantly, it will not bring more benefits. Other elements are compatible. By mixing the water, mixing the oil. and then coordinate by adding part of the oil into the water while spinning And in the last step add
Phospholipid into the formula and blend well.