Hello, I recommend using an electric stove. Gas stove, if needed, must be made as a double boiler, can not use direct fire Ingredient selection team From the members who have already selected, the water part
Aloe Vera Extract (อัตราสกัด 10:1 FullAssay™) 3%
Hyaluronic Acid Elastomer 10%
Ectoine (Ectoin) 2%
Ceramide Complex (CeraTouch™) 3 %
Vitamin B5 3%
Satin Cream Maker 1%
Mild Preserved Eco 1% (
สารกันเสีย ), water, the rest to complete 100% of the oil.
Jojoba Oil (Clear - Deodorized) 10%
shea butter 10%
Natural White Beeswax 5%
Butter Cream Maker 3% Discarded Items like other types of oil too light It will not be enough for a dry, peeling coating. Mixing process 1. To mix the water together. Without using heat. 2. To mix the oil together. Using heat at 70 degrees until the ingredients are dissolved together. 3. Bring the water to warm until the temperature is close to 70 degrees. 4. Gradually add the oil. into the water part By spinning or stirring continuously to combine. for newbies Please practice doing it little by little. to prevent damage If you mix it wrong